Creep testing machine

Creep testing machine

Make  : M/s. Spranktronics, Bangalore, India.

Application  :  Creep tests of polymers under tensile mode

Specification :

Load capacity :   up to 100 kg 

Data Acquisition System :   Measurement of load, displacement , temperature   with hardware  processing unit    and  time.

Software  :   Lab view software provides online plots of temperature-time vs load/displacement

Temperature range of the oven :  25°C  to 250°


Last updated on : 14-06-2018 03:24:46pm