Mechanical properties of titanium-titanium boride composites through nanoindentation...

Mechanical properties of titanium-titanium boride composites through nanoindentation...

Mechanical properties of titanium-titanium boride composites through nanoindentation and ultrasonic techniques an evaluation perspective, M. Selvakumar, P. Chandrasekar, B. Ravisankar, J. N. Balaraju, M. Mohanraj, Powder Metallurgy and Metal Ceramics, 53 (2015)  557-565, doi: 10.1007/s11106-015-9650-